ABSTRACT
Mode I stress
intensity factor was obtained by using electrical-resistance strain gages near
the crack tip of a 5083-0 aluminum made compact tension specimen as recommended
by ASTM standard E399. A theoretical method was also used to compare the results
with the experimental analysis. The results were in a good agreement up to the
critical stress concentration or beginning of crack propagation. The crack
opening started from 175 lb load application, and the mode I stress intensity
factor was about 7500 Psi (in)^0.5. The plastic zone size was also calculated
theoretically to determine the singularity dominated zone (SDZ). Send an email to request a copy of this paper.